Production And Forming Of Stainless Steel High Pressure Thick Wall Pipe Fittings And Elbows

Publish Time: Author: Site Editor Visit: 51

There are many production methods for Stainless Steel Weld Elbow. At the same time, the surface is divided into pickling, rolling sand and sandblasting. It can maintain a clean and tidy outer surface under some external conditions. Generally, the surface of seamless raw materials is selected according to the different production processes of steel pipes. In the chemical, petroleum, shipbuilding and natural gas industries, the demand for various seamless pipe fittings is very large. Therefore, it is precisely because the growth potential of the market is very large.

Aging treatment: In order to eliminate the changes in size and shape of precision measuring tools or molds and parts during long-term use, the workpiece is often reheated to ℃ after low-temperature tempering (low-temperature tempering temperature ℃) before finishing, and kept for 5-20 hours. This treatment to stabilize the quality of precision parts is called aging.

Aging treatment is performed on steel components under low temperature or dynamic load conditions to eliminate residual stress and stabilize the organization and size of hot-pressed elbows. Elbows are used for pipe fittings used to change the direction of pipeline turns. According to the angle, they are divided into 45-degree stainless steel elbows and 90-degree stainless steel elbows. To reduce the outer diameter, commonly used forging machines include rotary, connecting rod and roller types.

2. Rolling method: generally no mandrel is used, suitable for the inner round edge of thick-walled tubes.

Place a core in the tube, and use rollers to push the outer periphery for round edge processing.

3. Stamping method: Use a tapered core to expand the tube end to the required size and shape during punching.

4. Bending forming method: There are three commonly used methods, one is called stretching method, another is called stamping method, and the third is roller method, which has 3-4 rollers, two fixed rollers, and one adjustment roller. Adjust the fixed roller spacing, and the finished pipe fittings are bent.

Bulging method: One method is to place rubber in the tube, compress it with a punch on the top, so that the tube bulges out; the other method is hydraulic bulging forming, filling the middle of the tube with liquid, and the liquid pressure bulges the tube into the required shape. Most of the production of corrugated tubes uses this method. Hot forming technology is to heat the tube blank by induction heating to enhance the plasticity of the material.

Production And Forming Of Stainless Steel High Pressure Thick Wall Pipe Fittings And Elbows